defects[J]. Ocean Engineering, 2021, 222(1):108628.
2) *Mingming Sun(第一作者), Haisheng Zhao, Xin Li, et al. New evaluation method of failure pressure of steel pipeline with irregular-shaped defect[J]. Applied Ocean Research, 2021,110: 102601.
3) *Mingming Sun(第一作者), Xin Li, Jinkun Liu. Determination of folias factor for failure pressure of corroded pipeline[J]. Journal of Pressure Vessel Technology,2020,142(3):031802.
4) *Mingming Sun(第一作者), Yanfei Chen, Haisheng Zhao, et al. Analysis of
the impact factor of burst capacity models for defect-free pipelines[J]. International Journal of Pressure Vessels and Piping.
EI:
1) *孙明明(第一作者),李昕,李炜.海上风力机高桩承台基础反应特性研究[J].
太阳能学报,2020,41(07):265-273.
2) *孙明明(第一作者),李昕,刘锦昆.基于应变强化效应的管道流变应力分析[J].哈尔滨工程大学学报,2021, 42(01):89-95.
3) *孙明明(第一作者),李昕.基于膨胀系数修正的腐蚀管道失效压力预测[J].
中国造船,2021,62(02):68-81.
4) *孙明明(第一作者),李昕.不同屈服准则对完好管道失效压力的影响分析 [J].船舶力学,2021,25(11):1523-1532.
5) *孙明明(第一作者),李昕.环向对齐相邻缺陷管道失效压力研究[J].船舶力学,2022,26(07):1052-1063.
6) *孙明明(第一作者),方宏远,赵海盛,李昕.不规则缺陷管道失效压力影响因素及评价方法[J].中国石油大学学报(自然科学版),2022,46(04):152-159.
7) *孙明明(第一作者),赵海盛,方宏远,李昕.基于等效形状的不规则缺陷管道失效压力评估方法[J].表面技术,2022,51(08):319-329.
三、授权专利
发明型专利:
1) 李昕,*孙明明,彭增利,武行,张杰. 一种腐蚀管道 Folias 膨胀系数计算内压荷载的方法[P]. 辽宁省:CN108520135B,2020-05-19.
2) 李昕,*孙明明,武行,彭增利,张杰. 一种完好钢制管道极限内压的计算方法
[P]. 辽宁省:CN108562495B,2020-07-24.
3) 赵海盛,*孙明明,李昕. 一种不规则缺陷管道内压作用下的失效压力计算方法[P]. 辽宁省:CN112052609A,2020-12-08.
实用新型专利:
1)赵海盛 , 孙明明 , 李昕 . 一种 管道 内 压爆 破 装置 [P]. 辽 宁 省 :
CN214040955U,2021-08-24.
软件著作权:
1) 埋地管道地震反应分析软件 V1.0,登记号:2016SR283466
2) 集输管道极限内压计算分析软件 V1.0,登记号:2019SR1051959
3) 长距离有压管道失效压力计算软件 V1.0,登记号:2020SR0888144
4 ) 外压控制下含腐蚀缺陷海底管道压溃分析软件 V1.0 , 登记号:
2021SR0256888
5 ) 弯矩控制下平滑凹陷油气管道局部屈曲分析软件 V1.0 , 登记号:
2021SR0256851